This system is designed to recycle NMP from the lithium-ion secondary battery electrodes manufacturing process. The hot solvent laden air from the ovens is drawn into DRYAIR’s NMP Recovery System where the NMP is recovered by a combination of condensation and adsorption.The cleaned solvent laden air is available for return to the process or discharge to atmosphere as per customer requirement.NMP stands for N-Methyl-2-Pyrrolidone,it is an expensive solvent In addition, the recovery and recycling of NMP can reduce running costs for lithium battery factories as well as avoiding air pollution. Features : 97% recovery rate NMP discharge: 12ppm Conentration of recovered NMP Solvent:85% Functional section: Heat Ex-changer,Cooler VOC concentrator,Process fan Solvent Storage tank(optional) Siemens PLC
| ZJRH Series NMP Recovery System | ||||||
| Item | ZJRH-D30-9000 | ZJRH-D50-15000 | ZJRH-D60-20000 | ZJRH-D75-25000 | ZJRH-D90-30000 | ZJRH-D120-40000 |
| Process air volume CMH | 9000 | 15000 | 20000 | 25000 | 30000 | 40000 |
| NMP concentration in Discharged exhaust air | ≤50mg/m³ | |||||
| Concentration of Recovered NMP solvent | ≥85% | |||||
| NMP recovery rate | ≥97% | |||||
| Heat exchanger | efficiency≥65% | |||||
| Cooler#1 kw(≤32℃ chilling water) | 38 | 63 | 84 | 105 | 126 | 168 |
| Cooler#2 kw(≤10℃ chilled water) | 33 | 55.8 | 74 | 93 | 116 | 149 |
| Process fan #1 KW | 5.5 | 11 | 15 | 15 | 18.5 | 22 |
| Process fan #2 KW | 3 | 5.5 | 7.5 | 7.5 | 11 | 15 |
| Reactivation fan motor KW | 2.2 | 2.2 | 3 | 3 | 4 | 4 |
| Reactivation heate power KW | 12 | 18 | 22.5 | 27 | 36 | 48 |
| Rated power KW | 22.7 | 36.7 | 48 | 52.5 | 69.5 | 89 |